Wrought MMC Characteristics
Dense, refined microstructure after deformation processing
10-40% reinforcement typical (55% possible)
Focus on high structural properties
- Strength/Modulus
- Ductility/Toughness
- High Fatigue Resistance
Typically higher per pound cost